QA

We carry out a quality control of the production process in the following stages:

Before preservation:
Tree selection, humidity control and sizing.

During:
Finishes and preservation of the wood according to the technical specifications.

After:
Control of retention and penetration in accordance with current regulations. The retention is obtained by means of an X-ray spectrometer equipment.
TefQuim SA Provides the preservative Tanner-Wood CCAc, also verifies and controls the treatment of the Wood.
For quality control of preservative and Treated wood, the “SPECTRO PHOENIX” equipment is used.

Technical specifications:

For CCA it is guaranteed:

  • Total average retention kg. /m3 10.8
  • Maximum dampness content 30%
  • Penetration on the sapwood 100%
  • Salts balance:
Min. Cont. %Máx. Cont. %
Chrome44.550.5
Copper17.021
Arsenic
30.038.0

Our company works with the following Standards: IRAM 9513-9531-9597 ANSI 05.1 BRA-AWPA.